东莞市苏广塑胶原料有限公司
您当前的位置: 网站首页 > 产品展厅 >TPU-聚氨酯弹性体 聚酯型 聚醚 >高硬度TPU ELASTOLLAN 1174D
P 产品展厅RODUCT
高硬度TPU ELASTOLLAN 1174D
  • 品牌:1174D
  • 型号:1174D
  • 货号:88
  • 价格: ¥48/千克
  • 发布日期: 2023-06-16
  • 更新日期: 2025-02-14
产品详请
品牌 1174D
货号 88
用途 配件
牌号 1174D
型号 1174D
品名 TPU
包装规格 1174D
外形尺寸 7
生产企业 ARCS-60D
是否进口

Elastollan® 1174D

Thermoplastic Polyurethane Elastomer (Polyether)
BASF Corp. Thermoplastic Polyurethanes
产品说明:
Elastollan® 1174D exhibits excellent abrasion resistance, toughness, transparency, very good low temperature flexibility, hydrolytic stability and fungus resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® 1174D conforms to the FDA food contact regulations as described in book 21, section 177.2600 for wet food contact applications. Elastollan®1174D also has NSF Standard 61 "Water Contact Material" certification. Elastollan® 1174D is supplied uncolored in diced form.
物性信息:
基本信息
特性
  • 低温下的柔性
  • 良好的撕裂强度
  • 良好耐磨损性
  • 韧性良好
  • 食品接触的合规性
  • 水解稳定
机构评级
  • FDA 21 CFR 177.2600
  • NSF 61
外观
  • 清晰/透明
加工方法
  • 挤出
  • 注射成型
物理性能 额定值 单位制 测试方法
比重 1.19 g/cm3 ASTM D792
硬度 额定值 单位制 测试方法
肖氏硬度 (邵氏 D) 73 ASTM D2240
机械性能 额定值 单位制 测试方法
拉伸模量 (注塑) 524 MPa ASTM D412
弯曲模量 (注塑) 503 MPa ASTM D790
泰伯耐磨性 75.0 mg ASTM D1044
Abrasion - DIN 35 mm3 DIN 53516
热性能 额定值 单位制 测试方法
Softening Point - DMA 148 °C 内部方法
弹性体 额定值 单位制 测试方法
拉伸应力 ASTM D412
     应变 38.6 MPa ASTM D412
    300%应变 49.0 MPa ASTM D412
抗张强度 49.0 MPa ASTM D412
伸长率 (断裂) 300 % ASTM D412
撕裂强度 1 280 kN/m ASTM D624
压缩 变形 ASTM D395B
    23°C, 22 hr 40 % ASTM D395B
    70°C, 22 hr 60 % ASTM D395B
热性能 额定值 单位制 测试方法
玻璃转化温度 33.0 °C 内部方法
维卡软化温度 160 °C ASTM D1525
注射 额定值 单位制
干燥温度 110 到 120 °C
干燥时间 2.0 到 3.0 hr
建议的 水分含量 0.030 %
料筒后部温度 210 到 230 °C
料筒中部温度 210 到 230 °C
料筒前部温度 210 到 230 °C
射嘴温度 220 到 240 °C